Welcome to ‘Stainless Solutions’ from IMOA. Each month, we will cover a different stainless steel issue with tips on design and specification, and links to technical resources. This month’s issue will explore Whole Building Life Cycle Analysis (LCA) in voluntary rating systems and green codes. |
| Whole Building Life Cycle Analysis (LCA) |
|
Until recently, sustainable design mainly focused on building operation and interaction with its environment – energy and water use, community development, and health, safety and welfare. Decision makers know that construction material choice can significantly affect a project’s carbon footprint, but the only practical design option has been to specify longer life, more durable materials. A more complete building carbon footprint assessment was difficult, time consuming or even impossible because the necessary information and guidance were unavailable. Governments and advocates for more sustainable decision making have worked to remove those barriers to encourage more comprehensive carbon footprint assessment. Whole-building lifecycle assessment (LCA) standards, lifecycle inventory (LCI) databases, and software now make it possible to look at all phases of a building, from material extraction and production through construction to decommissioning and, where possible, recycling into a ‘new’ useful material. |
 |
The World Trade Center site in New York City is an excellent example of material durability concerns influencing decision-making. The One, Three and Seven World Trade Center buildings, the Goldman Sachs Headquarters, and the National September 11 Museum entrance all have Type 316L exteriors as will other projects around the site.
Photo credit Catherine Houska, TMR Consulting |
|
LCI data assesses the environmental impact of the production of each material. In LCA, the LCI data for each material is multiplied by the expected number of replacements over the service life of the project. There are LCI databases in Europe, Australia, the United States and elsewhere. There are finally enough materials in them, including all of the commonly used metals, for Whole Building LCA to be possible. |
 |
Government funded projects around the world increasingly have minimum design life requirements. Highly corrosion resistant 2205 duplex stainless steel sunscreens were used for the Stockholm Convention Center because of its coastal location.
Photo credit Outokumpu |
|
The third party certified LCI data used must be either from the individual supplier whose product is used or average data from the industry association in the specific country/region in which the material was produced because of energy source and environmental regulation differences. This is critical for a valid LCA analysis. Where databases have not yet been developed, Environmental Product Declarations (EPDs) from the producer or industry association can often provide the necessary information. Stainless steel is in these databases and many producers have EPDs. |
|
Proving its Long-term Mettle: Longevity, whole-building LCAs, and stainless steel,The Construction Specifier, provides more information on available resources, examples of stainless steel use in sustainable design and documentation of the material’s durability.
As resources become more developed, Whole Building LCA will become a regular part of sustainable design but, at this point, it is still optional in The International Green Construction Code (IgCC) and the most recent versions of the three widely used voluntary rating systems – US Green Building Council (USGBC) Leadership in Energy and Environmental Design (LEED), Green Star, and Building Research Establishment Environmental Assessment Method (BREEAM). |
|
Determining Material Replacement Frequency Material service life prediction is necessary for LCA. This may seem challenging but site assessment tools and comparative long-term corrosion testing data for metals are available. Here are a few resources to assist with that process:
Design & Selection Criteria
Comparative Metal Corrosion Data
Capabilities & Limitations of Architectural Metals
|
| Stainless Steel Library |
|
Download a free Stainless Steel Library (zip file, 559 MB) with over 360 pdfs covering building and construction applications, selection, specification, fabrication, sustainability and other common questions. |
| Stainless Solutions e-newsletter archive |
|
For previous issues or to subscibe to the e-newsletter, please visit the archive page. |
| Continuing Education – American Institute of Architects (AIA) |
|
IMOA is an AIA continuing education system approved provider with eight 1-hour programs that are registered for both live face-to-face and distance learning credit.
1. Stainless Steel Sustainable Design 2. Bioclimatic Design With Stainless Steel Weather Screens 3. Stainless Steel Structural Design 4. Stainless Steel Specification For Corrosive Applications 5. Deicing Salt: Stainless Steel Selection to Avoid Corrosion 6. Stainless Steel Finish Specification 7. Advanced Stainless Steel Specification and Problem Avoidance 8. Specification of Stainless Steel Finishes and Grades For Corrosive Applications
For more information or to schedule a workshop contact Catherine Houska, 412-369-0377 or email chouska@tmr-inc.com. |
| What is IMOA? |
|
IMOA (International Molybdenum Association) is a non-profit industry association, which provides technical information to assist with successful specification of molybdenum-containing materials. Molybdenum is an element. When it is added to stainless steel, molybdenum increases its resistance to corrosion caused by deicing salts, coastal atmosphere and pollution.
If you have a topic suggestion for a future issue of Stainless Solutions or need additional technical advice on stainless steel specification and selection, please get in touch here.
Forwarded by a colleague? To receive the next issue of Stainless Solutions automatically, please go to our archive and subscription page.
 
|
| Disclaimer |
|
In providing consultation or other assistance with respect to technical issues, any consultation, assistance or material is provided for the general information of the recipient and should not be used or relied upon for any specific application without first securing competent advice. IMOA and their respective employees, consultants and members (i) make no representation or warranty, express or implied, of any kind with regard to such consultation, assistance or material including no representation or warranty of suitability for any general or specific use; (ii) assume no liability or responsibility of any kind in connection therewith; and (iii) disclaim any and all liability for any claim that arises therefrom. |
|