Stainless Steel Selection System Case Studies

Case studies from around the world have been developed using IMOA's stainless steel selection system to explain instances of good performance and unacceptable corrosion staining. Download or order hardcopies of this literature here.

We are always adding new case studies. Please let us know if you have a project that we could use (info@imoa.info).

Case studies

Case Study 1: Pittsburgh and Chicago Handrails and Street Furniture
20/07/2009
Case Study 2: Minneapolis Exterior Wall Panels and Window Frames
19/07/2009
Case Study 3: New York and Miami Light Poles
18/07/2009
Case Study 4: Singapore Roofing
17/07/2009
Case Study 5: Hong Kong Building Exteriors and Railings
16/07/2009
Case Study 6: Canary Islands Railings and Lampposts
15/07/2009
Case Study 7: Barcelona Coastal Curtain Wall
14/07/2009
Case Study 8: Sao Paulo Building Exterior
13/07/2009
Case Study 9: Australian Costal Fence
12/07/2009
Case Study 10: New York Pier Railings
11/07/2009
Case Study 11: Thames Barrier
10/07/2009
Case Study 12: Milan Builden Exterior
09/07/2009
Case Study 13: Rio de Janeiro Building Exterior
08/07/2009
Case Study 14: New Zealand Coastal Building Exterior
07/07/2009