Press Releases
IMOA RELEASES NEW STATISTICS
15/02/2012
Global usage of molybdenum rose 15 per cent in the third quarter of 2011 compared with the same period in 2010 but fell compared with the previous quarter, according to new figures released this month by the...
STAINLESS STEEL USED IN INNOVATIVE BIOCLIMATIC SUSTAINABLE ARCHITECTURE
01/12/2011
In an article, published in the October issue of Construction Canada, IMOA consultant Catherine Houska discusses the new concepts involved in creating bioclimatic sustainable architecture including the new innovative...
TAIWAN STEEL SYMPOSIUM IS FIRST OF ITS KIND
02/11/2011
The International Molybdenum Association has joined forces with Taiwan National University, China Steel Corporation and niobium producer CBMM to organize the first steel symposium in Taiwan focusing on the synergies of...
MOLYBDENUM PRODUCTION AND USE RISES WORLDWIDE
01/09/2011
Global production of molybdenum rose by 14 per cent in the first three months of this year compared with the same period in 2010, according to figures released by the International Molybdenum Association (IMOA). China...
MOLYBDENUM USE HITS A NEW HIGH
13/06/2011
Global use of molybdenum has soared to a new high of 474 million lbs surpassing the peak use in 2007 of 470 million lbs, according to new full-year figures from the International Molybdenum Association. The greatest...
NEW RESEARCH HIGHLIGHTS FASTEST GROWING MARKETS FOR MOLYBDENUM
26/04/2011
New research by the International Molybdenum Association (IMOA) has highlighted power generation, building and construction and transportation as the three fastest growing markets for the global molybdenum industry...
MOLYBDENUM PRODUCTION ON THE RISE AS USAGE FALLS
14/02/2011
World-wide production of molybdenum continued to rise during the third quarter of 2010, although usage fell, figures released by the International Molybdenum Association (IMOA) reveal. In total, 132.2 million lbs of...
MORE STAINLESS STEEL ‘WEBINARS’ TO FOLLOW INITIAL SUCCESS
04/11/2010
Catherine Houska, a consultant to the International Molybdenum Association (IMOA) and one of the world’s leading experts in architectural metals, is planning a series of webinars – on-line tutorials –...
DUPLEX 2205 STAINLESS STEEL - CORROSION RESISTANCE FOR NUCLEAR POWER PLANTS
01/11/2010
Designers of cooling water systems for nuclear power plants now have an additional option when it comes to choosing corrosion resistant piping material. Piping in 2205 duplex stainless steel, which contains around 3.2...
MOLYBDENUM PRODUCTION RISES
28/10/2010
Global production of molybdenum rose in the second quarter of this year, figures released by the International Molybdenum Association (IMOA) show a total of 129.1 million lbs of molybdenum was produced, compared with...
IMOA ISSUES FIRST-EVER QUARTERLY STATISTICS
02/08/2010
The International Molybdenum Association (IMOA) has released quarterly production and use statistics for the first time ever. They show that in the first three months of this year (2010) 124.4 million lbs of Molybdenum...
MOLYBDENUM IS KEY TO FUTURE OF STEEL INDUSTRY, SEMINAR TOLD
30/06/2010
Improving the performance of steels through the use of molybdenum was the topic of a seminar in Beijing, the first of its kind ever held in China. Organised by the Beijing Antaike Information Development Co Ltd and...
MOLYBDENUM USE SET TO RISE AFTER GLOBAL FALL
28/06/2010
Worldwide production and use of molybdenum dropped significantly during 2009 because of the global recession, statistics released by the International Molybdenum Association (IMOA) show. Between 2005 and 2008,...
新闻发布
2010年6月28日18:00发布
据研讨会称:
钼对未来钢铁工业至关重要
通过使用钼来提高钢材性能是本次北京研讨会的主题,这是在中国首次举行的同类研讨会。
本次研讨会由北京安泰科信息开发有限公司承办,由钢铁研究总院(CISRI)和国际钼协(IMOA)主办,专家们研讨了目前的应用现状和未来的使用前景,同时重点探讨钼在钢中的特殊作用。
阅读详情