Stainless Steel Series
Stainless Steel Selection System Case Studies
Case studies from around the world have been developed using IMOA's stainless steel selection system to explain instances of good performance and unacceptable corrosion staining. Download or order hardcopies of this literature here.
We are always adding new case studies. Please let us know if you have a project that we could use.
Case Study 1: Pittsburgh and Chicago Handrails and Street Furniture (205 K)
- - - - - - - - - - - - - - - - - - -Case Study 2: Minneapolis Exterior Wall Panels and Window Frames (125 K)
- - - - - - - - - - - - - - - - - - -Case Study 3: New York and Miami Light Poles (140 K)
- - - - - - - - - - - - - - - - - - -Case Study 4: Singapore Roofing (170 K)
- - - - - - - - - - - - - - - - - - -Case Study 5: Hong Kong Building Exteriors and Railings (300 K)
- - - - - - - - - - - - - - - - - - -Case Study 6: Canary Islands Railings and Lampposts (140 K)
- - - - - - - - - - - - - - - - - - -Case Study 7: Barcelona Coastal Curtain Wall (120 K)
- - - - - - - - - - - - - - - - - - -Case Study 8: Sao Paulo Building Exterior (160 K)
- - - - - - - - - - - - - - - - - - -Case Study 9: Australian Coastal Fence (130 K)
- - - - - - - - - - - - - - - - - - -Case Study 10: New York Pier Railings (250 K)
- - - - - - - - - - - - - - - - - - -Case Study 11: Thames Barrier (195 K)
- - - - - - - - - - - - - - - - - - -Case Study 12: Milan Building Exterior (140 K)
- - - - - - - - - - - - - - - - - - -Case Study 13: Rio de Janeiro Building Exterior (145 K)
- - - - - - - - - - - - - - - - - - -Case Study 14: New Zealand Coastal Building Exterior (160 K)